Title: Cryogenic forming potential of large diameter and thin-walled aluminum alloy tubular materials
Authors: Sun, H 
Li, H
Yang, H 
Hao, XC
Liu, Y
Cong, RM
Fu, MW 
Issue Date: 2023
Source: In Mocellin, K, Bouchard, PO, Bigot, R, & Balan, T (Eds), Proceedings of the 14th International Conference on the Technology of Plasticity : Current Trends in the Technology of Plasticity : ICTP 2023 - Volume 4, p. 329-339. Cham, Switzerland: Springer, 2024.
Abstract: The large-diameter and thin-walled aluminum alloy tube has superiority in terms of weight reduction and high transmission efficiency which has been widely used in the aerospace field. However, it is a tough issue to deform a desirable bent tube with such extreme specification and small bending radius. In recent years, aluminum alloy materials have been found to show strong enhancement in both strength and ductility when deforms at cryogenic temperature (CT), which provide the cryogenic forming potential for the hard-to-bend aluminum alloy tubes. In this work, tube formability at room temperature (RT) and CT was explored. The anisotropic characterization of the thin-walled tube was realized by combining experiment and viscoplastic self-consistent (VPSC) model. The overall mechanical properties at CT are significantly improved compared to those at RT. Furthermore, a finite element model of cryogenic bending of the thin-walled 6061-O aluminum alloy tube was constructed. The results provide evidence from two aspects of wrinkling and wall thickness reduction that the thin-walled aluminum alloy tube difficult to form at RT can achieve better formability when bent at CT. The average wrinkle height decreases first from 1.182 mm at RT to 0.201 mm at −60 ℃ with 83.0% reduction, and then increases to 0.425 mm at −180 ℃. The average thickness reduction rate decreases monotonically with temperature decreasing, and the drop is fastest at −60 ℃ of 15.4% reduction. Cracks no longer appear in cryogenic bending. In terms of the effect on the two defects of wrinkling and wall thickness reduction, −60 ℃ is the temperature at which the best forming properties are obtained.
Keywords: Aluminum alloy
Anisotropy characterization
Cryogenic formability
Tube bending
Publisher: Springer
ISBN: 978-3-031-42092-4
978-3-031-42093-1 (eBook)
DOI: 10.1007/978-3-031-42093-1_32
Description: 14th International Conference on the Technology of Plasticity, Congress Center, Mandelieu, La Napoule, Bay of Cannes, France, September 24-29, 2023
Rights: © The Author(s), under exclusive license to Springer Nature Switzerland AG 2024
This version of the proceeding paper has been accepted for publication, after peer review (when applicable) and is subject to Springer Nature’s AM terms of use(https://www.springernature.com/gp/open-research/policies/accepted-manuscript-terms), but is not the Version of Record and does not reflect post-acceptance improvements, or any corrections. The Version of Record is available online at: http://dx.doi.org/10.1007/978-3-031-42093-1_32.
Appears in Collections:Conference Paper

Files in This Item:
File Description SizeFormat 
Sun_Cryogenic_Forming_Potential.pdfPre-Published version1.5 MBAdobe PDFView/Open
Open Access Information
Status open access
File Version Final Accepted Manuscript
Access
View full-text via PolyU eLinks SFX Query
Show full item record

Page views

73
Citations as of Apr 14, 2025

Downloads

12
Citations as of Apr 14, 2025

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.