Abstract: The effect of preheating treatment on NiAl compacts was systematically investigated. The preheating treatment of green compacts at 575 degrees C preserves their original shapes. The formation of porous NiAl alloys usually accompanies with the volume expansion due to the formation of Ni(2)Al(3) during the preheating treatment. The pore structures of porous NiAl alloys strongly depended on the preheating duration. The volume expansion, porosity and the maximum pore size increased with prolonged preheating treatment duration. Whereas the maximum pore size of final product decreased with increased preheating treatment duration. It has been found that the pore structures especially the maximum pore size strongly depend on the volume expansion determined by the intensity of exothermic reaction from the preheating temperature to the finally sintering temperature.
URI: http://hdl.handle.net/10397/8259
ISSN: 0925-8388
DOI: 10.1016/j.jallcom.2009.12.018
Appears in Collections:Journal/Magazine Article

Access
View full-text via PolyU eLinks SFX Query
Show full item record

SCOPUSTM   
Citations

8
Citations as of Nov 2, 2017

WEB OF SCIENCETM
Citations

5
Last Week
0
Last month
0
Citations as of Nov 16, 2017

Page view(s)

41
Last Week
1
Last month
Checked on Nov 13, 2017

Google ScholarTM

Check

Altmetric



Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.