Title: (Na0.475K0.475Li0.05)(Nb 0.92Ta0.05Sb0.03)O3lead-free ceramics with addition of CeO2
Authors: Lee, T
Kwok, KW 
Chan, HLW 
Issue Date: 2007
Source: IEEE International Symposium on Applications of Ferroelectrics, 2007, 4393364, p. 667-669 How to cite?
Abstract: Lead-free piezoelectric ceramics (Na0.475K 0.475Li0.05)(Nb0.92Ta0.05Sb 0.03)O3 added with different amounts of CeO2 have been prepared by a conventional mixed-oxide method. After the addition of CeO2, the sintering performance of the ceramics is greatly improved. The ceramics can be well-sintered at a higher temperature, and hence have a higher density and better piezoelectric and dielectric properties. For the ceramic added with 0.4 wt% CeO2, the piezoelectric and dielectric properties become optimum, giving d33 = 246 pC/N, kp = 0.50, εr= 1300 and tanδ= 4%.
Description: 2007 16th IEEE International Symposium on the Applications of Ferroelectrics, ISAF, Nara-city, 27-31 May 2007
URI: http://hdl.handle.net/10397/31782
ISBN: 1424413338
9781424413331
DOI: 10.1109/ISAF.2007.4393364
Appears in Collections:Conference Paper

Access
View full-text via PolyU eLinks SFX Query
Show full item record

Page view(s)

35
Last Week
1
Last month
Checked on Aug 13, 2017

Google ScholarTM

Check

Altmetric



Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.