Title: Dielectric behaviour and polarization response of proton irradiated Ba 0.65Sr0.35TiO3/P(VDF-TrFE) composites
Authors: Adikary, SU
Chan, HLW 
Choy, CL 
Sundarvel, B
Wilson, IH
Keywords: 0-3 Polymer/ceramic composites
Barium strontium titanate
Polyvinylidene fluoride-trifluoroethylene
Proton irradiation
Relaxor-ferroelectrics
Issue Date: 2002
Source: Japanese journal of applied physics, Part 1 : Regular papers and short notes and review papers, 2002, v. 41, no. 11 B, p. 6938-6942 How to cite?
Journal: Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers 
Abstract: Ba0.65Sr0.35TiO3/P(VDF-TrFE)70/30 composites have been prepared by dispersing Ba0.65Sr 0.35TiO3 powder in a vinylidene fluoride-trifluoroethylene copolymer (with 70 mol% vinylidene fluoride) matrix. The effects of irradiation with 3 MeV protons on the dielectric properties and polarization response of the composites have been investigated. At a dosage of 100 Mrad, both the copolymer and the composites exhibit a broad peak in the relative permittivity whose location shifts upwards in temperature with increasing frequency. This result implies that the proton irradiation breaks up the coherent polarization domains in the normal ferroelectric copolymer phase into nanopolar regions, thereby converting the material to a relaxor ferroelectric. The polarization-electric field hysteresis loop becomes slimmer after irradiation, particularly for the composites with low ceramic volume fraction. For the unirrdiated samples, the slight increase of remnant polarization with ceramic volume fraction indicates that the remnant polarization of the ceramic phase is not much higher than that of the copolymer phase. After irradiation, the remnant polarization of the copolymer drops sharply. The remnant polarization of the irradiated composites rises steeply with increasing ceramic volume fraction and is only 20% lower than that of the unirradiated composites at a ceramic volume fraction of about 0.5.
URI: http://hdl.handle.net/10397/25768
ISSN: 0021-4922
DOI: 10.1143/JJAP.41.6938
Appears in Collections:Journal/Magazine Article

Access
View full-text via PolyU eLinks SFX Query
Show full item record

SCOPUSTM   
Citations

6
Last Week
0
Last month
0
Citations as of Mar 24, 2017

WEB OF SCIENCETM
Citations

7
Last Week
0
Last month
0
Citations as of Mar 19, 2017

Page view(s)

21
Last Week
0
Last month
Checked on Mar 19, 2017

Google ScholarTM

Check

Altmetric



Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.