Title: The morphology of solidification of thin-section ductile iron castings
Authors: Yeung, CF
Zhao, H
Lee, WB 
Issue Date: 1998
Publisher: Elsevier
Source: Materials characterization, 1998, v. 40, no. 4-5, p. 201-208 How to cite?
Journal: Materials characterization 
Abstract: The morphology of solidified structures of thin-section ductile iron castings has been investigated by color metallographic techniques. Primary austenitic dendrites were observed to be formed over the whole section of castings when the wall thickness was less than 14mm. The dendrites were thin and long, and the length and the number of dendrites depended on the solidification rate or the wall thickness of the casting. Growth of the dendritic arms was directional, being perpendicular to the surface of castings and along the wall thickness. Interdendrite segregation of Si and Mn is found to occur in thin-section ductile iron castings, as revealed by both color metallography and energy dispersive X-ray microanalysis. The segregation is more pronounced toward the center of castings.
URI: http://hdl.handle.net/10397/20604
ISSN: 1044-5803
DOI: 10.1016/S1044-5803(98)00012-6
Appears in Collections:Journal/Magazine Article

Access
View full-text via PolyU eLinks SFX Query
Show full item record

SCOPUSTM   
Citations

18
Last Week
0
Last month
0
Citations as of Aug 19, 2017

WEB OF SCIENCETM
Citations

18
Last Week
0
Last month
0
Citations as of Aug 20, 2017

Page view(s)

34
Last Week
3
Last month
Checked on Aug 20, 2017

Google ScholarTM

Check

Altmetric



Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.